NewAI Part GeneratorFree to get started
FREE TOOL

PCB trace resistance calculator

Get a trace's DC resistance, voltage drop and power loss from its width, length, copper weight, temperature and current. This PCB trace resistance calculator also works backward from an allowed voltage drop to the width or length that meets it.

Solve for
Examples
Units
mm
mm
°C

Ambient plus any self-heating.

A

Optional: voltage drop and power loss.

Trace resistance

200.9 mΩ

Sheet resistance
0.5023 mΩ/sq
Number of squares (L ÷ w)
400
Resistance per mm
2.009 mΩ/mm 51.03 mΩ/in
Resistance at 20 °C
197 mΩ
Voltage drop at 1 A
200.9 mV
Power loss
200.9 mW
Current density
114 A/mm²

This is DC resistance with uniform current. Above about 3.6 MHz, where the skin depth equals this copper thickness, AC resistance starts to climb.

Resistance against width, 100 mm long at 25 °C
10m100m10.050.10.20.512Trace width (mm)Resistance (Ω)0.25 mm
0.5 oz1 oz2 oz

The same trace in other copper weights

CopperResistanceDropPower loss
0.5 oz401.8 mΩ402 mV402 mW
1 oz200.9 mΩ201 mV201 mW
2 oz100.5 mΩ100 mV100 mW
3 oz66.97 mΩ67 mV67 mW

How do you calculate PCB trace resistance?

Use R = ρ × L ÷ (w × t), with copper resistivity 1.7241 × 10⁻⁸ Ω·m at 20 °C. The resistance rises 0.393 % per °C. A trace 0.25 mm wide and 100 mm long in 1 oz (35 µm) copper is 201 mΩ at 25 °C, or 2.01 mΩ per mm.

PCB trace resistance formula

A trace is a rectangular copper bar, so its DC resistance follows from the resistivity of copper and its cross-section.

R(T) = ρ₂₀ × (1 + α × (T − 20)) × L ÷ (w × t)
R(T)
resistance in Ω at temperature T
ρ₂₀
resistivity of annealed copper at 20 °C, 1.7241 × 10⁻⁸ Ω·m
α
temperature coefficient at 20 °C, 0.00393 per °C
L, w, t
trace length, width and copper thickness in m

Splitting off the copper gives the sheet resistance, which is handy for layout estimates:

Rs = ρ ÷ t     R = Rs × (L ÷ w)

The drop and the loss at current I, and the width for an allowed drop V:

V = I × R     P = I² × R     w = ρ × L × I ÷ (t × V)

How to calculate PCB trace resistance: worked examples

Example 1: a 100 mm signal trace at 25 °C

1 oz copper has Rs = 0.502 mΩ/sq at 25 °C. A 0.25 mm wide, 100 mm long trace is 400 squares, so R = 201 mΩ. At 500 mA it drops 100 mV and dissipates 50.2 mW.

Example 2: width for a 50 mV drop at 3 A over 40 mm

The target is 50 mV ÷ 3 A = 16.7 mΩ. With 2 oz copper at 60 °C, Rs is 0.285 mΩ/sq, so w = Rs × L ÷ R = 0.684 mm. IPC-2221 needs 0.449 mm on an outer layer for a 20 °C rise at 3 A, so here the voltage drop sets the width. On an inner layer IPC-2221 asks for 1.17 mm, and heating takes over.

Example 3: the same trace at 85 °C

Raising the copper from 25 °C to 85 °C takes the trace in example 1 from 201 mΩ to 247 mΩ, an increase of 23.1 %.

PCB trace resistance per mm

Milliohms per millimeter of length at 25 °C, using 35 µm per ounce of copper.

Width0.5 oz1 oz2 oz3 oz
0.1 mm (3.94 mil)105.022.511.67
0.15 mm (5.91 mil)6.73.351.671.12
0.2 mm (7.87 mil)5.022.511.260.837
0.25 mm (9.84 mil)4.022.0110.67
0.3 mm (11.8 mil)3.351.670.8370.558
0.5 mm (19.7 mil)2.0110.5020.335
1 mm (39.4 mil)10.5020.2510.167
2 mm (78.7 mil)0.5020.2510.1260.0837
5 mm (197 mil)0.2010.10.05020.0335

Sheet resistance of PCB copper

In mΩ per square, for the copper weights fabs quote and the temperatures boards see.

Temperature0.5 oz1 oz2 oz3 oz
20 °C0.9850.4930.2460.164
25 °C10.5020.2510.167
50 °C1.10.5510.2750.184
85 °C1.240.6180.3090.206
105 °C1.310.6570.3290.219
125 °C1.390.6960.3480.232

How thin finished copper can be

Minimum inner-layer thickness after processing (IPC-A-600J Class 2, as published by Eurocircuits), and what it does to the resistance at 25 °C.

Nominal copperMinimum finishedSheet resistance, nominalSheet resistance, minimumIncrease
18 µm11.4 µm0.977 mΩ/sq1.54 mΩ/sq57.9 %
35 µm24.9 µm0.502 mΩ/sq0.706 mΩ/sq40.6 %
70 µm55.7 µm0.251 mΩ/sq0.316 mΩ/sq25.7 %
105 µm86.6 µm0.167 mΩ/sq0.203 mΩ/sq21.2 %

Where the simple model stops

The formula assumes uniform DC current in a rectangular section of annealed copper. Etched traces are slightly trapezoidal, and electrodeposited copper can have a somewhat higher resistivity than the annealed standard, so treat the result as a best case. 35 µm per ounce is the fab convention; foil makers target 34.3 µm with a 10 % tolerance. Outer layers are plated up from a thinner starting foil, so their thickness varies with the process. Short, wide runs are dominated by current spreading at the pads and vias, which this model ignores. Self-heating raises the resistance too: enter the copper temperature, not the ambient, for a trace carrying real current. NBS Circular 31 takes the resistance of copper as linear up to 200 °C and probably from −100 °C to 300 °C, and the calculator warns outside that range.

Glossary

Sheet resistance
Resistance of any square of a conductive sheet, ρ ÷ t, in ohms per square.
Square
One unit of length ÷ width. A trace 100 mm long and 0.25 mm wide is 400 squares.
Copper weight
Foil specified by mass per area: 1 oz/ft² is about 35 µm thick.
Finished copper
Thickness after processing and plating, which differs from the nominal foil.
Temperature coefficient (α)
Fractional change in resistance per °C: 0.00393 for copper at 20 °C.
Skin depth
The depth at which AC current density falls to 1/e of its surface value.

Related guides

Frequently asked questions

How do you calculate the resistance of a PCB trace?

R = ρ × L ÷ (w × t), with copper resistivity ρ = 1.7241 × 10⁻⁸ Ω·m at 20 °C. Multiply by 1 + 0.00393 × (T − 20) for other temperatures. A 100 mm long, 0.25 mm wide trace in 1 oz copper is 201 mΩ at 25 °C.

What is the sheet resistance of 1 oz copper?

0.502 mΩ/sq at 25 °C for 35 µm copper. Multiply it by the number of squares (length ÷ width) to get the trace resistance.

What is the resistance of a 10 mil trace per inch?

50.2 mΩ per inch in 1 oz copper at 25 °C. Half-ounce copper doubles that and 2 oz halves it.

How much does temperature change trace resistance?

About 0.393 % per °C of the 20 °C value. Going from 25 °C to 85 °C raises the resistance by 23.1 %.

Does trace resistance change with frequency?

Yes. The skin depth in copper is about 66.1 µm at 1 MHz, and once it falls to the copper thickness (around 3.6 MHz for 1 oz) current crowds toward the surface and AC resistance rises above the DC value here.

Why does my measured trace resistance differ from the calculation?

Mostly copper thickness. Finished copper is not the nominal figure: a 1 oz inner layer can be as thin as 24.9 µm and still meet IPC-A-600J Class 2, which raises the resistance by 40.6 %. Measure with four wires so that probe resistance does not add to a milliohm reading.

How do I reduce the voltage drop across a trace?

Widen it, shorten it or use heavier copper; resistance scales with L ÷ (w × t). Doubling the width halves the drop. For high currents use a pour or a plane, and parallel vias at each layer change.

Can I use this as a PCB trace voltage drop calculator?

Yes. Enter the current and it returns the drop, V = I × R, and the loss, P = I² × R. A 0.25 mm wide, 100 mm long trace in 1 oz copper at 500 mA and 25 °C drops 100 mV and dissipates 50.2 mW.

What resistivity does a copper trace resistance calculator use?

This one uses 1.7241 × 10⁻⁸ Ω·m at 20 °C for annealed copper, from NBS Circular 31, and scales it by 1 + 0.00393 × (T − 20) for other temperatures. Electrodeposited copper can have a somewhat higher resistivity, so treat the result as a best case.

More free PCB tools

See all free electronics tools →

Sources

Design the whole board, not one number

ProtoFlow is free AI PCB design software: describe a circuit and get a schematic with real parts, PCB layout with an autorouter, SPICE simulation and Gerber files. Native KiCad, Altium and EAGLE import and export. Free on macOS, Windows and Linux.

Get for Mac

Free to start. No card required.